Cobalt Chrome Alloy Sheet
Cobalt Chrome Alloy
- TNM
- China
- 20 days
- 2000pcs/month
- Information
1. Cobalt alloys have higher melting points than nickel (or iron) alloys ,This gives them the ability to absorb stress to a higher absolute temperature .
2. Cobalt alloys give superior hot corrosion resistance to gas turbine atmospheres , this is due to their high chromium content.
3. Cobalt alloys show superior thermal fatigue resistance and weldability over nickel alloys .
---Excellent wear and corrosion resistance even at high temperature up to 800℃
SYTOP cobalt base alloys is a range of cobalt-chromium-tungsten alloys with wear resistance, corrosion and high thermal resistance. It is widely used in oil & gas, machinery, wood cutting, automotive, paper and food processing industry etc.
Chemical compositions and properties (%)
Brand | C | Mn | Si | Cr | Ni | Mo | W | Co | Fe | P | S | Density (g/cm3) | Hardness (HRC) |
Cobalt Chrome Alloy3 | 2.0-2.7 | 1.0 | 1.0 | 29-33 | 3.0 | 11-14 | Bal. | 3.0 | ≤0.03 | ≤0.03 | 8.55 | 51-55 | |
Cobalt Chrome Alloy 6 | 0.9-1.4 | 1.0 | 1.5 | 27-31 | 3.0 | 1.5 | 3.5-5.5 | Bal. | 3.0 | ≤0.03 | ≤0.03 | 8.35 | 38-44 |
Cobalt Chrome Alloy 12 | 1.1-1.7 | 1.0 | 1.0 | 28-32 | 3.0 | 7.0-9.5 | Bal. | 3.0 | ≤0.03 | ≤0.03 | 8.40 | 44-49 | |
Cobalt Chrome Alloy 20 | 2.2-3.0 | 2.0 | 30-34 | 3.0 | 1.0 | 14-18 | Bal. | 3.0 | ≤0.05 | ≤0.05 | 8.65 | 53-59 | |
Tantung-G 25 | 2.2-2.8 | 1-3 | 27-32 | 7 | Ta/Nb | 14-19 | Bal. | 2-5 | 8.84 | 57-60 | |||
Tantung-G35 | 3.3-3.8 | 1-3 | 27-32 | 7 | Ta/Nb | 14-19 | Bal. | 2-5 | 8.80 | 60-63 | |||
Tribaloy 400 | 0.04 | 2.5-2.7 | 8-10 | 27-29 | Bal. | 55 | |||||||
Tribaloy 800 | 0.04 | 3.2-3.6 | 16-18 | 27-29 | Bal. | 58 |
Specifications that we can made :
Different size bars , rods , ingots , plate
Drawing made seal , valve seat and ball , bush and sleeve etc.
Some size tube
Most of our products are made upon request so contact us right now for personal and professoinal service .